DataSheet.es    


PDF PN0906 Data sheet ( Hoja de datos )

Número de pieza PN0906
Descripción SMD Power Inductors Unshielded
Fabricantes Premo 
Logotipo Premo Logotipo



Hay una vista previa y un enlace de descarga de PN0906 (archivo pdf) en la parte inferior de esta página.


Total 6 Páginas

No Preview Available ! PN0906 Hoja de datos, Descripción, Manual

www.DataSheet4U.com
PN0906



















































 SMD
Power
Inductors
Unshielded
C/Severo Ochoa 33 – Parque Tecnológico de Andalucía. 29590 Campanillas .Málaga (Spain) Phone +34 951 231 320 Fax +34 951 231 321
E-mail: [email protected] Web http://www.grupopremo.com
1. Configuration & Dimensions
Series
PN0906
A
9.5±0.5
B(max.)
10.5
2. Schematic Diagram
Dimensions [mm]
C EF
6.0±0.3
2.5±0.3 11.0±0.5
F’
12.7±0.8
W(typ.)
0.6
3. Materials
a.- Core : Ferrite DR Core
b.- Wire : Enamelled copper wire (class F)
c.- Base : LCP E4008
d.- Terminal : Cu / Sn
e.- Adhesive : Epoxy resin
f.- Remark : Lead content 200ppm max. include ferrite
1
SMD
Power
Inductors

















































P R E M O
All rights reserved. Passing on of this document, use and communication of contents not permitted without written authorisation.

1 page




PN0906 pdf
www.DataSheet4U.com
PN0906



















































 SMD
Power
Inductors
Unshielded
C/Severo Ochoa 33 – Parque Tecnológico de Andalucía. 29590 Campanillas .Málaga (Spain) Phone +34 951 231 320 Fax +34 951 231 321
E-mail: [email protected] Web http://www.grupopremo.com
Style
Dimensions [mm]
AB CDGNT
13 – 24
330
21±0.8
13±0.5
24
26+0 50-0 30.4
Series
PN0906
Q’TY(pcs)
600
8. Labelling
Inner : Reel
G.W.(gw)
1,400
Style
13 – 24
Outer : Carton
Q’TY(pcs)
G.W.(Kg)
Size(cm)
2,400
7.6 40 x 40 x 24
9. Reliability Test
Test item
Solderability
Specification
Test condition
More than 90% of the
terminal electrode
shall be covered
with fresh solder
Preheat : 150±25% for 60 seconds
Solder : Sn96.5 / Ag3 / Cu0.5 or equivalent
Solder temp. : 235±5ºC
Flux : Rosin
Dip time : 4±1 seconds
Thermal shock test
(Temp. cycle)
Inductance shall
not change more
than ±20%
Room temp.
15 minutes
Room temp.
15 minutes
Total : 50 cycles
-25±2ºC
30 minutes
85±2ºC
30 minutes
Humidity
Resistance test
Temperature : 40±2ºC
Humidity : 90 ~ 95%
Applied current : Per specifications
Time : 500 hours
High temp.
Resistance test
Temperature : 105±2ºC
Applied current : Per specifications
Time : 500 hours
5
SMD
Power
Inductors

















































P R E M O
All rights reserved. Passing on of this document, use and communication of contents not permitted without written authorisation.

5 Page










PáginasTotal 6 Páginas
PDF Descargar[ Datasheet PN0906.PDF ]




Hoja de datos destacado

Número de piezaDescripciónFabricantes
PN0906SMD Power Inductors UnshieldedPremo
Premo

Número de piezaDescripciónFabricantes
SLA6805M

High Voltage 3 phase Motor Driver IC.

Sanken
Sanken
SDC1742

12- and 14-Bit Hybrid Synchro / Resolver-to-Digital Converters.

Analog Devices
Analog Devices


DataSheet.es es una pagina web que funciona como un repositorio de manuales o hoja de datos de muchos de los productos más populares,
permitiéndote verlos en linea o descargarlos en PDF.


DataSheet.es    |   2020   |  Privacy Policy  |  Contacto  |  Buscar